The same times and temperatures as for 
development can be used for fixing. The actual 
fixing time, however, is shorter, and 20 seconds is 
ample above 20ºC/68ºF. These recommendations 
are suitable for both replenished and 
MULTIGRADE IV RC 
 
 
MACHINE PROCESSING 
MULTIGRADE IV RC paper can be processed in all 
conventional machines for black and white resin 
coated papers. It is not suitable, however, for 
activation type processing. 
 
ILFORD processors 
ILFORD 2000RT developer/replenisher and 
fixer/replenisher are recommended for use with all 
ILFORD black & white processors. 
 
For the ILFOLAB 2150RC table-top processor 
ILFORD 2150XL developer and fixer kits are 
recommended. 
 
Other processors 
This section is a guide to setting up processors for 
ILFORD resin coated papers using ILFORD 2000RT 
developer/replenisher and fixer/replenisher. These 
are diluted 1+4 to make tank or replenisher 
solution. These suggestions are only a guide, and 
the processing cycle should be checked in the 
processor. For further guidance, contact your local 
ILFORD company or distributor. 
 
Suggested development times 
The preferred temperature range is 20–30ºC/ 
68–86ºF. 
 
Temperature 
Development time (sec) 
(ºC/ºF) 
including transfer time to next tank 
20/68 46 
25/77 32 
30/86 22 
35/95 15 
40/104 12 
 
These times are for non-replenished systems, with a 
maximum solution life of seven days. They are also 
for replenished systems with a solution life of up to 
three months. The suggested developer 
replenishment rate is 150–250ml/m
(14–23ml/ft
2
) paper processed. 
 
Suggested fixing times 
non-replenished systems. In non-replenished 
systems, the maximum paper throughput is 4m
2
/l 
(44ft
2
/US quart) of working strength solution. The 
suggested fixer replenishment rate for replenished 
systems is 300–450ml/m
(28–41ml/ft
2
) of paper 
processed. The maximum silver concentration in 
the fixer bath is 4–6g/l. 
 
Note If fixing is not complete, then adequate 
washing is impossible. 
Washing times 
Wash for at least 15 seconds at temperatures 
above 5ºC/41ºF. Set the water flow so as to fill 
the wash tank in 4 minutes or less. 
 
Hot air drying 
Use temperatures up to 85ºC/185ºF. 
 
FINISHING 
MULTIGRADE IV RC responds in the same way as 
other resin coated papers to the usual techniques 
of toning, chemical reduction and retouching. It 
can be mounted using the standard techniques for 
resin coated papers. 
 
STORAGE 
Unprocessed paper 
Store unused MULTIGRADE IV RC paper in a cool, 
dry place in its original packaging. Avoid 
conditions of high temperature and/or high 
humidity. MULTIGRADE IV RC will keep in excellent 
condition for up to two years when stored as 
recommended. 
 
Prints 
MULTIGRADE IV RC prints which have been 
processed as recommended in this leaflet will have 
a more than adequate storage life for most 
purposes. Print life will be shortened, however, in 
adverse storage conditions, or if the print is 
exposed to oxidising gases. 
 
It is recommended that prints made for display are 
toned to protect them from the oxidising gases that 
are found in many environments. Selenium toner is 
recommended as it has little effect on the image 
colour of MULTIGRADE IV RC, but other protection 
methods can be used including sulphide toning, 
silver image stabilisers and laminating. ILFORD 
ILFOGUARD laminating and encapsulating films 
are recommended. 
 
A wide range of fact sheets is available which describe and 
give guidance on using ILFORD products. Some products in 
this fact sheet might not be available in your country. 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
HARMAN 
technology Limited, Ilford Way, 
Mobberley, Knutsford, Cheshire WA16 7JL, England  
www.ilfordphoto.com
 
 
 
 
 
 
 
Page 4 of 4 
 
           June 2010