WELD DIAGNOSIS
ExCESS OR BURN-THROUGH
Weld droops on top and 
underneath, or falls through 
entirely, making a hole.
PROPER
Weld is visible underneath and 
bulges slightly on top.
INADEqUATE
Weld does not contact the joint 
fully, just on the surface.
WELD PENETRATION
POSSIBLE CAUSES AND SOLUTIONS
1. 
Excessive material at weld: 
Reduce wire feed speed.
2. 
Overheating: 
Increase welding speed and ensure that 
welding speed is kept steady.
POSSIBLE CAUSES AND SOLUTIONS
1. 
Workpieces too thick/close: 
Joint design must allow weld to reach bot-
tom  of  groove  and  allow  proper  welding 
procedures.
2. 
Incorrect welding technique: 
Maintain 
1
/
2
” or less stickout. 
Keep  arc  on  leading  edge  of  weld  pud-
dle. 
Hold gun at proper angles as stated under 
Holding The Torch on page 17.
3. 
Insufficient weld material: 
Increase wire feed speed.
4. 
Insufficient weld heat: 
Reduce Welding Speed.
Cross seCtIons
WELD  NOT  ADHERING  PROPERLY
Gaps present between weld and previous bead or 
between weld and workpiece.  See areas below.
POSSIBLE CAUSES AND SOLUTIONS
1. 
Dirty workpiece: 
Make certain that workpiece is clean and 
free  from  oil,  coatings,  and  other  resi-
dues.
2. 
Insufficient weld material: 
Increase wire feed speed.
3. 
Incorrect welding technique: 
Place  stringer  bead  at  correct  place  in 
joint. 
Adjust workpiece position or weld angle to 
permit proper welding to bottom of piece. 
Pause briefly at sides when using a weave 
bead. 
Keep  arc  on  leading  edge  of  weld 
puddle. 
Hold gun at proper angles as stated under 
Holding The Torch on page 17.
Cross 
seCtIon
BEND AT jOINT
POSSIBLE CAUSES AND SOLUTIONS
1. 
Improper clamping: 
Make  sure  that  pieces  are  clamped  se-
curely in place. 
Make tack welds to help hold pieces.
2. 
Excessive heat: 
Weld  a  small  portion  and  allow  to  cool 
before proceeding. 
Reduce wire feed speed. 
Increase weld speed. 
Cross 