Road Condition Durability Testing
Third Party Testing of the Unconstrained Design
To prove the durability of the unconstrained design, 3M sent two trailers to the
Bosch Automotive Proving Grounds in South Bend, Indiana. The side panels on
one test trailer were attached with 3M
VHB
Tapes. Panels on the other test trailer
were mechanically fastened. An independent test team at Bosch performed durability
testing over various road conditions and exposure to heat cycling. 
Testing parameters for heat cycle 
and road condition durability
Instruments were attached inside 
each trailer to detect changes in 
side panel position or dynamics
Trailers were overloaded 120%
Series of road tests simulated 
hauling 100,000 miles
After the 100,000 mile road test, a
pressure washer set at 3200 PSI sprayed
water over each seam of the smooth-sided
trailer. No leaks were detected. 3M
VHB
Tapes bond and seal in one step,
helping reduce or eliminate the sealants
required with mechanically-fastened
panels.
Result: After a simulated 100,000 miles of different road conditions
non-constrained panel construction held tight preventing leaks, absorbing 
vibration, and reducing noise. 33% of the mechanical fasteners were 
loose at 36,000 miles.