symptom
possible Cause
possible solution
Fuzzy grain.
1.  Workpiece  has  high  moisture  content  or 
surface wetness.
2.  dull knives/inserts.
1.  sticker  and  allow  workpiece  to  dry  if  moisture 
content is over 20% or has surface wetness.
2.  sharpen/replace knives (
Page 36).
long lines or ridges 
that run the length 
of the workpiece.
1.  nicked or chipped knife.
1.  sharpen/replace knives (
Page 36).
uneven cutting 
marks, wavy 
surface, or chatter 
marks across 
the face of the 
workpiece.
1.  Feed rate too fast.
2.  Chip breaker or pressure bar set unevenly.
3.  one  or  both  of  the  bed  rollers  are  set  too 
low or too high.
4.  Knife heights not correct.
5.  Worn cutterhead bearings.
1.  reduce feed rate (
Page 25).
2.  Adjust the height of the chip breaker or pressure bar 
(
Page 40).
3.  lower/raise the bed rollers (
Page 26).
4.  Adjust knives to the proper height (
Page 36).
5.  replace cutterhead bearings.
glossy surface.
1.  Knives are dull.
2.  Feed rate too slow.
3.  depth of cut too shallow.
1.  sharpen/replace knives (
Page 36).
2.  increase feed rate (
Page 25).
3.  increase depth of cut (
Page 26).
inconsistent chip 
marks.
1.  Chips are not being properly expelled from 
around the cutterhead.
1.  use an adequate dust collection system; adjust the 
chip deflector in or out, depending upon your setup 
(
Page 43).