9.6. Vibration Strength (in individual packing) 
There shall be no sign of malfunction after the following vibration test. 
Vibration test: 
Increase the frequency of the vibration from 10Hz to 100Hz at an accelerated 
velocity of 19.6 m/s
2
 (2.0 G) for 30 minutes (60 minutes per cycle) in individually packaged state. 
Repeat this in each X, Y and Z direction.  
 
9.7. Drop Impact Strength (without packaging) 
There shall be no sign of malfunction after the following drop test. 
Drop test:
 Drop the scanner 30 times in total (5 times at each 6 face) from a height of 150 cm onto 
a concrete floor as shown below.  
150cm
 
 
Figure 10: Drop Test 
 
9.8. Drop Impact Strength (in individual packaging) 
There shall be no sign of malfunction after the following drop test. 
Drop test:
 Drop an individually packaged scanner 10 times in total, at any of 1 corner, 3 edges, and 
6 faces, from a height of 150 cm onto a concrete floor. 
 
9.9. Electrostatic Discharge (ESD) Immunity  
Contact discharge 
 
: ±6 kV max (direct or indirect discharge, no malfunction) 
Aerial discharge 
: ±8 kV max (no malfunction) 
  ±15 kV max (no distraction) 
 
 
Measurement environment   : Testing method compliant with IEC-61000-4-2. 
Discharge resistance 
: 330 Ω 
Charging capacitor 
: 150 pF 
 
Concret